0.5Ba0.7Ca0.3TiO3 – 0.5BaZr0.2Ti0.8O3 thin films with varying thicknesses have been deposited on Pt/Si and quartz substrates by pulsed laser deposition to investigate the influence of thickness and oxygen vacancies on their structural, optical and functional properties. The deposited films exhibit the coexistence of tetragonal-P4mm and rhombohedral-R3m phases with progressive strain relaxation as thickness increases. Increasing thickness promotes island-like growth with enhanced grain coalescence and surface roughness, while reduces the oxygen vacancy concentration, leading to higher Ti4+/Ti3+ and lattice oxygen fractions. The work function increases from 4.94 to 5.07 eV due to a downward Fermi-level shift and reduced band bending, whereas the optical bandgap narrows from 3.77 to 3.58 eV owing to suppressed Burstein–Moss shift and strain relaxation. Increase in thickness shows a downward shift of both VBM and EF (confirmed from valence band XPS). Photoluminescence intensity decreased due to reduced defect density and improved crystallinity. Piezoresponse force microscope reveals enhanced ferroelectric domain stability with an increase d33 from 49 to 78.5 pm/V observed. Leakage current density decreased by nearly three orders of magnitude with Schottky emission identified as the dominant conduction mechanism. Overall, film thickness effectively tunes oxygen stoichiometry, electronic structure, ferroelectric and electrical properties in 0.5BCT–0.5BZT thin films.