Speaker
Description
Thin films of Mo(W)Sex composite were grown on molybdenum (Mo) substrates through a single-step process combining RF magnetron sputtering of tungsten (W) with simultaneous thermal evaporation of selenium (Se). Growth temperature was varied from room temperature (RT) to 300℃, to investigate the influence on film properties. Surface morphological analysis (FESEM) showed dense coalescing features at RT, which evolved to a continuous flake like network at 100℃. Beyond this temperature, the surface coverage transitioned to rarefied dot-like features pointing towards a progressive decline in deposit density. EDX analysis showed negligible W incorporation despite continuous sputtering, while the Se content decreased with increase in temperature. XRD and Raman spectroscopy indicated that the crystallinity observed at 100℃ was predominantly associated with trigonal Se and Mo3Se4, with no clear evidence of targeted WSe2/MoSe2 phases. The Se depletion at higher temperatures can be attributed to thermally driven Se re-evaporation and enhanced oxygen incorporation. I–V measurements showed a systematic decrease in threshold voltage with increasing growth temperature. Cyclic voltammetry, carried out at 40 mV/s in acidic media resulted in a non-ideal capacitive response. Although the targeted WSe2 phase was not achieved, the results demonstrate a clear relationship between growth temperature, chalcogen retention, composition, and electrical/electrochemical behaviour. This will act as a basis for further optimization of W and Se fluxes.